Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Zone 1 | 180 °C | 356 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Zone 1 | 180 °C | 356 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Zone 1 | 180 - 195 °C | 356 - 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Zone 1 | 180 °C | 356 °F | |
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 1 | 180 °C | 356 °F | |
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 1 | 180 °C | 356 °F | |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 1 | 180 °C | 356 °F | |
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | Injection |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Star L POM D11 POM, Injection Molded Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Star L POM D84 POM, Injection Molded Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam MF0044 PP, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam MF0044 is a Halogen Free Flame Retardant, Glass Fiber Reinforced, PP Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | |
Lubrizol Estane® 54601 Thermoplastic Polyurethane Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A.. |