| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant | 
| Manufacturer | Eurostar Engineering Plastics | 
| Trade Name | Starflam | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 | 
| Water Absorption | 0.010 % @Temperature 23.0 °C, Time 86400 sec | 0.010 % @Temperature 73.4 °F, Time 24.0 hour | ISO 62-1 | 
| Linear Mold Shrinkage, Flow | 0.016           cm/cm @Thickness 4.00 mm | 0.016           in/in @Thickness 0.157 in | E2P method | 
| Melt Flow | 10           g/10 min @Load 5.00 kg, Temperature 230 °C | 10           g/10 min @Load 11.0 lb, Temperature 446 °F | ISO 1133 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength at Break | 25.0 MPa | 3630 psi | 50 mm/min; ISO 527 | 
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 | 
| Elongation at Yield | 7.3 % | 7.3 % | 50 mm/min; ISO 527 | 
| Flexural Yield Strength | 50.0 MPa | 7250 psi | 2 mm/min; ISO 178 | 
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 | 
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80x10x4; ISO 180/1A | 
| Izod Impact, Unnotched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80x10x4; ISO 180/1U | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow | 106           µm/m-°C @Temperature 23.0 - 60.0 °C | 58.9           µin/in-°F @Temperature 73.4 - 140 °F | ISO 11359-2 | 
| CTE, linear, Transverse to Flow | 140           µm/m-°C @Temperature 23.0 - 60.0 °C | 77.8           µin/in-°F @Temperature 73.4 - 140 °F | ISO 11359-2 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf | 
| Deflection Temperature at 1.8 MPa (264 psi) | 57.0 °C | 135 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af | 
| Flammability, UL94 | V-2 @Thickness 1.60 mm | V-2 @Thickness 0.0630 in | |
| Glow Wire Test | 850           °C @Thickness 1.60 mm | 1560           °F @Thickness 0.0630 in | IEC 60695-2-12 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Zone 1 | 180 - 190 °C | 356 - 374 °F | |
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Zone 3 | 190 - 200 °C | 374 - 392 °F | |
| Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
| Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
| Drying Temperature | 70.0           °C @Time 10800 sec | 158           °F @Time 3.00 hour |