Processing Properties Metric English Comments
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LL1091 LLDPE  (discontinued **)
Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LL1091-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM112-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM115-B LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature 149 °C
300 °F
Hopper Temperature
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)  (Unverified Data**)
Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Alathon® M5370WC High Density Polyethylene
ApplicationsALATHON M 5370WC is a natural, high density, polyethylene copolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cab..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® KR92717 High Density Polyethylene
ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® KR92828 High Density Polyethylene
ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont..
Feed Temperature 149 °C
300 °F
Extrusion
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
Feed Temperature 149 °C
300 °F
Extrusion
Huntsman IROGRAN® CA116-205 TPU-Polyester
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR590001 High Density Polyethylene
ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR590005 High Density Polyethylene
ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains ..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR686001 High Density Polyethylene
ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen..
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LL1091-AS LLDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LL1092-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM115-C LLDPE  (discontinued **)
Additives: Medium Antiblock, Low SlipFeatures: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM124-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM203-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM213-C LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Feed Temperature <= 149 °C
<= 300 °F
M. Holland Company MAGMA® LM233-A LLDPE  (discontinued **)
Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland.