| Category | Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | M. Holland Company MAGMA® LM124-C LLDPE
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
| Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Elongation at Break, MD | 900 % | 900 % | ASTM D882 |
| Film Elongation at Break, TD | 1000 % | 1000 % | ASTM D882 |
| Elmendorf Tear Strength MD | 450 g | 450 g | ASTM D1922 |
| Elmendorf Tear Strength TD | 500 g | 500 g | ASTM D1922 |
| Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
| Film Tensile Strength at Break, MD | 42.1 MPa | 6100 psi | ASTM D882 |
| Film Tensile Strength at Break, TD | 37.2 MPa | 5400 psi | ASTM D882 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 97.2 °C | 207 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 1.8 % | 1.8 % | ASTM D1003 |
| Gloss | 90 % | 90 % | at 45°; ASTM D2457 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | <= 149 °C | <= 300 °F | |
| Zone 1 | 149 °C | 300 °F | |
| Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
| Blow-up Ratio (BUR) | 2.0 - 3.0 | 2.0 - 3.0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets |