Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Drying Temperature | 100 - 140 °C @Time 7200 - 14400 sec |
212 - 284 °F @Time 2.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |