Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. Non flammable.High chemical resistance parts.High dimensionally stable precision parts with low warpage and narrow tolerance range.Gear parts for automotive appliances, body parts, grippers, spacers.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ISO 1183
Water Absorption <= 0.20 %
<= 0.20 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 160 MPa
23200 psi
Elongation at Yield 1.5 %
1.5 %
2.0 %
2.0 %
flexural
Modulus of Elasticity 13.0 GPa
1890 ksi
Flexural Strength 225 MPa
32600 psi
Flexural Modulus 11.0 GPa
1600 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
220 °C
428 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 320 - 340 °C
608 - 644 °F
Zone 1 300 - 320 °C
572 - 608 °F
Zone 2 310 - 330 °C
590 - 626 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color blue