Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7336/GY7016 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8179 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8432 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8496 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Drying Temperature | 150 °C @Time >=14400 sec |
302 °F @Time >=4.00 hour |
or |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Drying Temperature | 150 °C @Time 10800 - 18000 sec |
302 °F @Time 3.00 - 5.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7327 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7583 PEEK, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Chemical and hydroly.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7709/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7740 PEEK, lubricant modified, heat stabilized Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Drying Temperature | 150 °C @Time 10800 - 21600 sec |
302 °F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |