Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 30.0 - 124 MPa | 4350 - 18000 psi | Average value: 93.1 MPa Grade Count:13 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Injection Pressure | 30.0 - 100 MPa @Time 2.00 - 10.0 sec |
4350 - 14500 psi @Time 0.000556 - 0.00278 hour |
|
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner JEPP2007 PP For Automotive Parts Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner JEPP2056 PP For Automotive Parts Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Zhejiang Juner JEPPB003 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner PP201-G30 PP For Automotive Parts Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner PP6-1JE PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 45.0 MPa | 4350 - 6530 psi | |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | (DAM) |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Injection Pressure | 30.0 MPa | 4350 psi | Recommended Molding Pressure. |
Asahi Glass Fluon® G307 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Injection Pressure | 30.0 MPa | 4350 psi | Recommended Molding Pressure. |
Asahi Glass Fluon® G340 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Injection Pressure | 30.0 - 55.0 MPa | 4350 - 7980 psi | |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 MPa | 4350 psi | Recommended Molding Pressure. |
Asahi Glass Fluon® G350 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |