Material Notes:
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Bulk Density 0.820 g/cc
0.0296 lb/in³
Particle Size 350 µm
350 µm
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Diametrical Shrinkage
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
JIS K6891
Elongation at Break 350 %
350 %
JIS K6891
Processing Properties Metric English Comments
Injection Pressure 30.0 MPa
4350 psi
Recommended Molding Pressure.
Descriptive Properties Value Comments
Compression Ratio 2.5