Polymer Property : Injection Pressure = 82.7 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 55.2 - 82.7 MPa
8000 - 12000 psi
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
PTS Trilac® ABS-HS7500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
TPI Porene® ABS-GA800 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
TPI Porene® ABS-KU650 Super High Heat ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
Chi Mei Polylac® PA-747 ABS
High impact