Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Barrel Temperature |
SABIC PP 5701P Polypropylene Homopolymer for Injection Molding Product Description: PP 5701P is specially for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Barrel Temperature |
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Barrel Temperature |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | Recommended injection moulding temperature |
Reliance Industries Relene M60075 Polyethylene Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade.. |
|||
Processing Temperature | 220 - 230 °C | 428 - 446 °F | C2 |
UBE 5033B Air Blown Nylon 6/66 Film Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | C4 |
UBE 7024B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | C4 |
UBE 7034B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Total HDPE SB 1461 High Density Polyethylene - Injection Stretch Blow Molding HDPE SB 1461 is a high density polyethylene with very high stiffness. It has been specifically designed for the manufacture of thin walled containers for foodstuffs (dairy applications particularly.. |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | |
Zhejiang Juner PA-A6-1 MF25% Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | |
Zhejiang Juner PA-A6-3 GF/MF Reinforced Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 220 °C | 428 °F | C3 |
UBE 7024B Five Layer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Range |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 240V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | Resin Temperature |
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Range |
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | Injection molding cylinder temperature |
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |