Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7197/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8157 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8356 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Processing Temperature | 390 - 425 °C | 734 - 797 °F | |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0904/GN PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7596/BL PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/40 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 - 425 °C | 734 - 797 °F | |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |