Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 20808 Polyvinylidene Fluoride (PVDF) Copolymer; Low ViscosityAdditional Properties: Abrasion Resistance - ASTM D4060 29.0 mg; Coefficient of Friction - ASTM D1894 0.280; Coefficient of Linear Thermal Expansion - ASTM D696 1.4E-4 to 1.6.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 25.0 °C |
0.382 BTU/lb-°F @Temperature 77.0 °F |
solid; DSC |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 25.0 °C |
0.382 BTU/lb-°F @Temperature 77.0 °F |
solid; DSC |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 25.0 °C |
0.382 BTU/lb-°F @Temperature 77.0 °F |
solid; DSC |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E968 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM C351 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |