Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastman AP005 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastman
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastman AP005 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPolymer modificationProfilesRubber and plastic modificationSporting goodsThermoplastic elastomer compoundsTubingKey Attributes:Environmentally preferred, non-halogenated materialExcellent chemical and oil resistanceExcellent compatibility with a wide range of polymersExcellent processabilityExceptional heat resistance and high temperature dimensional stabilityHigh energy absorptionHigh flexibility without plasticizersMelt bondable to a variety of substrates, including PVCOutstanding toughness and puncture resistanceSolvent bondableProduct Description: Eastman AP005 is a tough, clear, durable copolyester ether that combines the strength of plastics, the flexibility of elastomers, and the processability of thermoplastics. Eastman AP005 can be used in injection molding and film or tubing extrusion applications or in any application that demands strength, durability, chemical resistance, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, high temperature resistance and flexibility without the addition of plasticizers. Eastman AP005 is considered environmentally preferred because of its non-halogenated material composition. Its broad compatibility with other polymers such as styrenic block copolymers makes it an excellent choice for both alloys and as additives/modifiers to improve performance properties.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 0.35 %

@Time 86400 sec
0.35 %

@Time 24.0 hour
Immersion; ASTM D570
Water Vapor Transmission 132 g/m²/day
8.50 g/100 in²/day
ASTM F372
Oxygen Transmission Rate 841 cc/m²/day

@Pressure 0.101 MPa,
Temperature 30.0 °C
54.2 cc/100 in²/day

@Pressure 14.7 psi,
Temperature 86.0 °F
ASTM D1434
Viscosity Measurement 1.05
1.05
Inherent; EMN-A-AC-G-V-1
Thickness 130 microns
5.12 mil
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Film Tensile Strength at Yield, MD 13.7 MPa
1990 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.5 MPa
1960 psi
ASTM D882
Tensile Strength, Yield 14.0 MPa
2030 psi
ASTM D638
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Film Elongation at Yield, MD 26 %
26 %
ASTM D882
Film Elongation at Yield, TD 26 %
26 %
ASTM D882
Elongation at Break 300 %
300 %
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Flexural Modulus 0.150 GPa
21.8 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm

@Temperature -40.0 °C
0.937 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Coefficient of Friction >= 1.0
>= 1.0
ASTM D1894
Tear Strength, Total 370 N
83.2 lb (f)
ASTM D1004
Film Tensile Strength at Break, MD 23.7 MPa
3440 psi
ASTM D882
Film Tensile Strength at Break, TD 22.6 MPa
3280 psi
ASTM D882
Tangent Modulus 179 MPa
26000 psi
T.D.; ASTM D882
185 MPa
26800 psi
M.D.; ASTM D882
Torsional Stiffness 240 MPa

@Temperature -28.0 °C
34800 psi

@Temperature -18.4 °F
ASTM D1043
930 MPa

@Temperature <=-70.0 °C
135000 psi

@Temperature <=-94.0 °F
ASTM D1043
Thermal Properties Metric English Comments
Heat of Fusion 27.0 J/g
11.6 BTU/lb
ASTM E793
CTE, linear 150 µm/m-°C
83.3 µin/in-°F
ASTM D696
Specific Heat Capacity 1.60 J/g-°C

@Temperature 25.0 °C
0.382 BTU/lb-°F

@Temperature 77.0 °F
solid; DSC
1.80 J/g-°C

@Temperature 100 °C
0.430 BTU/lb-°F

@Temperature 212 °F
solid; DSC
2.00 J/g-°C

@Temperature 150 °C
0.478 BTU/lb-°F

@Temperature 302 °F
solid; DSC
2.30 J/g-°C

@Temperature 175 °C
0.550 BTU/lb-°F

@Temperature 347 °F
solid; DSC
2.30 J/g-°C

@Temperature 225 °C
0.550 BTU/lb-°F

@Temperature 437 °F
melt; DSC
3.10 J/g-°C

@Temperature 200 °C
0.741 BTU/lb-°F

@Temperature 392 °F
transition; DSC
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 207 °C
405 °F
Crystalline Peak; ASTM D3418
Crystallization Temperature 140 °C
284 °F
DSC
Vicat Softening Point 170 °C

@Load 1.00 kg
338 °F

@Load 2.20 lb
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Glass Transition Temp, Tg -3.00 °C
26.6 °F
DSC
Optical Properties Metric English Comments
Refractive Index 1.51
1.51
n<sub>D</sub>; ASTM D542
Haze 1.0 %
1.0 %
for Film; ASTM D1003
Gloss 80 %
80 %
for Film, 45°; ASTM D2457
Transmission, Visible 90 %

@Thickness 0.130 mm
90 %

@Thickness 0.00512 in
Regular, Film; ASTM D1003
93 %

@Thickness 0.130 mm
93 %

@Thickness 0.00512 in
Total, Film; ASTM D1003
Users viewing this material also viewed the following: