Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics GELOY XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Hot Ball Pressure Test | 95.0 - 100 °C | 203 - 212 °F | Average value: 95.6 °C Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East) NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN.. |
|||
Hot Ball Pressure Test | 95.0 °C | 203 °F | IEC 60335-1 |
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 320U Acrylonitrile Butadiene Styrene Saxalac 320U is an UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 340Q Acrylonitrile Butadiene Styrene Saxalac 340Q is an siliconized, UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tes.. |
|||
Hot Ball Pressure Test | <= 95.0 °C | <= 203 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX .. |
|||
Hot Ball Pressure Test | 95.0 °C @Thickness 2.00 mm |
203 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |