Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 96.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 96.0 °C

@Load 5.10 kg
205 °F

@Load 11.2 lb
ISO 306/B 120
Polimeri Europa Sinkral® PD L 322 ABS Resin
Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and..
Vicat Softening Point 96.0 °C

@Load 5.001 kg
205 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYasa 1614F UV-resistant ASA
Information provided by Polykemi AB
Vicat Softening Point 96.0 °C

@Load 5.001 kg
205 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH FR15030 XNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa H-12 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa HR-527 Modified ABS
Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 96.0 °C

@Load 1.02 kg
205 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution PS 486N HIPS
Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution..
Vicat Softening Point 96.0 °C

@Load 5.10 kg
205 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Terluran® HI-12 ABS
Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution
Vicat Softening Point 96.0 °C

@Load 5.10 kg
205 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
Vicat Softening Point 96.0 °C

@Load 5.10 kg
205 °F

@Load 11.2 lb
ISO 306
Borealis HK060AE Polypropylene Homopolymer
HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr..
Vicat Softening Point 96.0 °C

@Load 5.10 kg
205 °F

@Load 11.2 lb
ISO 306
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh impact resistance at low temperature, high gloss, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene
ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 96.0 °C

@Load 0.999 kg
205 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HG 0808 Polystyrene
High gloss polystyreneHigh impact resistance, good physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-726 ABS
Electro-plating
Vicat Softening Point 96.0 °C

@Load 1.00 kg
205 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
High impact
Vicat Softening Point 96.0 °C

@Load 1.00 kg
205 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer
Injection Molding, High rigidity
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-727 ABS
Electro-plating
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756 ABS - High Flow
High rigid, high flow
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-756S ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 96.0 °C

@Load 5.00 kg
205 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-763 ABS - Flame Retardant
F.R. High Heat Weather Resistant
Vicat Softening Point 96.0 °C

@Load 1.00 kg
205 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-33 Polystyrene
Standard grade
Vicat Softening Point 96.0 °C

@Load 1.00 kg
205 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PG-80 Polystyrene
High strength