Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 436 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 570H-10 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8172 (829) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8511R (853RP-2) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8511U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512SC (842S-CP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8530 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8730 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8971 (898-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8971R (898RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering V71C Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Terpolymer of vinylidene difluoride and hexafluoropropylene tetrafluoroethylene. Compounded to have extremely low temperature capability, Glass transition tem.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering V97B Fluoroelastomer Compound Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Wher.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC method |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Heat Resistance; ASTM D570D |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |