Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended |
Nye Lubricants 731B (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended |
Nye Lubricants UniFlor 8711 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended use; SAE J-2236 |
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V60G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = colour gr.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V70A Fluoroelastomer Compound Blue Fluoroelastomer Rubber, 65-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2, where Z1 = comp-.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Dow Corning SE 4448 CV KIT PARTS A&B Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous use |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | few hours; VDE 0304/P2-1, IEC 216 |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | few hours; VDE 0304/P2-1, IEC 216 |
EPICHEM PA 66 Polyamide 66 |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Chosun Refractories APC-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Dow Corning XIAMETER® PMCPPMX-200 1000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 1,000CS. 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a .. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Mechanical per UL Card E54153 |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579GA028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Maximum Service Temperature, Air | >= 200 °C | >= 392 °F | 2 hours |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | rated per UL card E54153 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Maximum Service Temperature, Air | 200 °C @Time >=1200 sec |
392 °F @Time >=0.333 hour |
|
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method. Application: Composition is intended to be processed into pressure pipes.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |