Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
Nye Lubricants 704C (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
Nye Lubricants UniFlor 8122 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Precision Polymer Engineering E80B Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistan.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
Nye Lubricants 786A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 150 - 160 °C | 302 - 320 °F | Average value: 157 °C Grade Count:6 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Maximum Service Temperature, Air | 150 °C @Thickness 3.0 mm |
302 °F @Thickness 0.12 in |
UL Temperature Index |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Intermittent |
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Dow Corning 7096 CLEAR SEALANT Clear, neutral cure, multi-purpose silicone adhesive/sealant.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | long term; EMS |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | long term; EMS |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous use |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous use |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Short Periods |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | long term; EMS |
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | Service |
3M FM069 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
3M 853 Polyester Tape 3M™ Polyester Tape 853 is comprised of strong, thin polyester backing with high shear, solvent resistant acrylic adhesive. These qualities make this tape ideal for applications where solvent exposu.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Maximum Service Temperature, Air | 150 °C | 302 °F | |
Hydrogenated Nitrile Rubber (HNBR) |