Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
Continuous |
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Deflection Temp.; ASTM D648 |
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W-KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 HS-GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; DIN 52612 |
Isoflon PC Polycarbonate Good impact resistance among transparent materialsInformation provided by Isoflon. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Styrolution Luran® S KR 2863 C Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek PA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond 2170T Flexible Plastic Bonder TRA-BOND 2170T is a flexible, high viscosity, thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or alm.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond F125 Fast Gel Clear Epoxy Adhesive TRA-BOND F125 is a 10 minute gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. This clear, two part system is easily mixed and used at room te.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Trelleborg E566 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Trelleborg E569 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Trelleborg E666 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | short term; EMS |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Deflection temperature; load unknown |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Service |
3M FMV02 Void Polyester Label Products 3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Long Term |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond 868-6N3 Room Temperature Cure Epoxy Adhesive TRA-BOND 868-6N3 room temperature cure epoxy is a thixotropic version of TRA-BOND 868-6N1 adhesive. This adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, bra.. |