Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting properties such as: Outstanding impact resistance even at low temperaturesHigh flexural fatigue resistanceResistance to a wide range of solvents and chemicalsExcellent stress crack resistanceLow densityExcellent weathering resistanceLight opacity allows various colours Grilamid TR 90 NZZ natural is suitable for technically demanding parts such as safety and sports spectacles and can be processed in injection moulding and extrusion technologies.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Water Absorption 3.0 %
3.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eA
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 70.0 - 90.0 °C
158 - 194 °F
long term; EMS
115 °C
239 °F
short term; EMS
Transformation Temperature, Tg 155 °C
311 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 45.0 kV/mm
1140 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Exterior
Fuel systems
Interior
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Optics Spectacle frames
Processing Injection Molding
Other Extrusion
Product Attributes Co Polyamide
Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved