Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | Average value: 115 °C Grade Count:3 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Maximum Service Temperature, Air | 105 - 130 °C | 221 - 266 °F | Average value: 124 °C Grade Count:5 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage toleran.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix HexPly® M47 is a toughened, self extinguishing 140ºC curing epoxy resin matrix that has been developed for the performance car market. It exhibits good strength retention at elevated temperature, .. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg 42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel |
|||
Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is .. |
|||
Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610.. |
|||
Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSG-60 PA666-GF60 Product description: Grilon TSG-60 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers. Grilon TSG-60 has the following important properties: Very high st.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 3959 nat PA610 Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4073 nat PA610 Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materi.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4105 black 9992 PA610-GF50 Product description: Grilamid XE 4105 black 9992 is a 50% glass fiber reinforced, heat stabilized and UV resistant polyamide 610 (PA610) injection molding grade. This product is to a large extent ba.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | |
Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLongest pot lifeLarges.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 60.0 - 130 °C | 140 - 266 °F | Average value: 92.7 °C Grade Count:14 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |