| Category | Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite | 
| Manufacturer | Hexcel | 
| Trade Name | HexPly® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield |           920           MPa           @Temperature 23.0 °C  | 
                  133000           psi           @Temperature 73.4 °F  | 
        0º, Conditioning: 23°C; ASTM D3039 | 
| Tensile Modulus |           60.0           GPa           @Temperature 23.0 °C  | 
                  8700           ksi           @Temperature 73.4 °F  | 
        0º, Conditioning: 23°C; ASTM D3039 | 
| Flexural Yield Strength |           935           MPa           @Temperature 90.0 °C  | 
                  136000           psi           @Temperature 194 °F  | 
        0º, Conditioning: 23°C; ASTM D790 | 
|           950           MPa           @Temperature 23.0 °C  | 
                  138000           psi           @Temperature 73.4 °F  | 
        0º, Conditioning: 23°C; ASTM D790 | |
| Flexural Modulus |           40.0           GPa           @Temperature 90.0 °C  | 
                  5800           ksi           @Temperature 194 °F  | 
        0º, Conditioning: 23°C; ASTM D790 | 
|           43.0           GPa           @Temperature 23.0 °C  | 
                  6240           ksi           @Temperature 73.4 °F  | 
        0º, Conditioning: 23°C; ASTM D790 | |
| Compressive Yield Strength |           537           MPa           @Temperature 90.0 °C  | 
                  77900           psi           @Temperature 194 °F  | 
        0º, Conditioning: 23°C; ASTM D965 | 
|           715           MPa           @Temperature 23.0 °C  | 
                  104000           psi           @Temperature 73.4 °F  | 
        0º, Conditioning: 23°C; ASTM D965 | |
| Shear Strength |           39.0           MPa           @Temperature 60.0 °C  | 
                  5660           psi           @Temperature 140 °F  | 
        0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344 | 
|           57.0           MPa           @Temperature 90.0 °C  | 
                  8270           psi           @Temperature 194 °F  | 
        0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 | |
|           80.0           MPa           @Temperature 23.0 °C  | 
                  11600           psi           @Temperature 73.4 °F  | 
        0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Shelf Life |           12.0           Month           @Temperature -18.0 °C  | 
                  12.0           Month           @Temperature -0.400 °F  |