Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WEJB400LU Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 4167 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Features: High Gloss; Sunlight Resistant (720 hours)Uses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW; SJT; SRDT; ST; SVT Agency Ratings: UL QM.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 1001 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Heat Resistance Value at 2 psi. |
Valley Adhesives EM-490 High Temperature Application Glue Stick Valley Adhesives EM-490 High Temperature Application Glue StickExcellent tack; Used on plastics, metals and other surfaces. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | See Note 2. |
ChevronTexaco Crater® Fluid M Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M 7047 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FA03J Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP024402 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products FP024402 and FP024408 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra remova.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP032302 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP032305 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP0862 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP08R2 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP531 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP532 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV092R Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV094 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV517 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FVT44 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FA021 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP025409 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are clear materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tac.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FS502 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV023205 White Vinyl Label Products 3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV02800N Textured Vinyl Label Products 3M™ Textured Vinyl Label Products are flexible and conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212 which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV02940N Textured Vinyl Label Products 3M™ Textured Vinyl Label Products are flexible and conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212 which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV037 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Maximum Service Temperature, Air | 60.0 - 130 °C | 140 - 266 °F | Average value: 92.7 °C Grade Count:14 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |