Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 325 °C | 617 °F | |
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.Advantages & Appl.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® 8900 Fluoroelastomer DuPont™ Kalrez® 8900 perfluoroelastomer parts are a black product for all thermal processes, e.g., oxidation, diffusion furnace, metal CVD, ALD and LPCVD. It offers outstanding thermal stability, .. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® AeroSeal™ 7777 Fluoroelastomer DuPont™ Kalrez AeroSeal™ 7777 perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257C. It offers outstanding thermal stab.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® AeroSeal™ 7797 Fluoroelastomer DuPont™ Kalrez AeroSeal™ 7797 perfluoroelastomer parts are a specialty black product specifically targeted for use in applications requiring high hardness/higher modulus properties. It offers outs.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® AeroSeal™ 7800 Fluoroelastomer Kalrez AeroSeal™ 7800* perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257. It offers outstanding thermal stability and.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® PV8070 Fluoroelastomer DuPont™ Kalrez® PV8070 perfluoroelastomer parts are a black product for PV cell manufacturing processes requiring high temperature resistance including doping for n-type layer formation (bulk c-Si.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | DuPont Test Method |
DuPont Performance Polymers Kalrez® Spectrum™ 7090 Fluoroelastomer DuPont™ Kalrez Spectrum™ 7090 perfluoroelastomer parts are specifically targeted for use in applications requiring high hardness/higher modulus properties. These specialty black parts have excelle.. |
|||
Maximum Service Temperature, Air | 325 °C | 617 °F | Intermittent |
Atom Adhesives AA-DUCT 904 Epoxy Adhesive AA-DUCT 904 is a single component, heat curing, conductive epoxy that was designed for ease in handling. This high performance conductive epoxy cures quickly at elevated temperatures making it ideal.. |