DuPont Performance Polymers Kalrez® 8900 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 8900 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Kalrez® 8900 perfluoroelastomer parts are a black product for all thermal processes, e.g., oxidation, diffusion furnace, metal CVD, ALD and LPCVD. It offers outstanding thermal stability, very low outgassing and excellent (low) compression set properties. Kalrez® 8900 parts exhibit excellent retention of physical properties at elevated temperatures, have excellent mechanical strength and are well-suited for both static and dynamic sealing applications. A maximum continuous service temperature of 325 °C is suggested. Short excursions to higher temperatures may also be possible. Ultrapure post-cleaning and packaging is standard for all Kalrez® 8900 parts. Features/Benefits Outstanding thermal stability Excellent (low) compression set properties Very low outgassing properties Very low moisture content Excellent retention of physical properties at elevated temperatures Excellent resistance to fluorine gas Suggested Applications Quartz Tube Seals Plenum Seals Chamber Seals Fittings Center Ring Seals .
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Pellet; ASTM D2240
Hardness, Shore M 82
82
O-ring; ASTM D1414, ASTM D2240
Tensile Strength at Break 20.75 MPa
3010 psi
ASTM D412
Elongation at Break 137 %
137 %
ASTM D412
100% Modulus 0.01221 GPa
1.771 ksi
ASTM D412
Compression Set 9.0 %

@Temperature 204 °C,
Time 252000 sec
9.0 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
32 %

@Temperature 300 °C,
Time 252000 sec
32 %

@Temperature 572 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
59 %

@Temperature 325 °C,
Time 252000 sec
59 %

@Temperature 617 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 325 °C
617 °F
DuPont Test Method
Descriptive Properties Value Comments
Color Black