Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlast® G75B has been specially formulated to provide increased acid resistance by eliminating fillers that are prone to acid attack and optimising the polymer structure. In addition, this perfluoroelastomer has low permeability and as a result, it is less prone to swelling, leading to extended in-service performance in, for example, valves, pumps and mechanical seals. A high modulus makes G75B resistant to extrusion and ideal for use in high pressure environments. In addition, the low long-term compression set provides a high mean-time between maintenance cycles in hot chemically aggressive environments. Perlast® G75B is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.Applications: Aerospace: Inter-stage seal assemblies (static O-rings). Chemical Processing: Pumps; Valves; Mechanical seals. Diesel: Cylinder bore liners (static O-rings); Exhaust valve seats. Semiconductor: Gas abatement systems (static); High vibration environments. Oil & Gas: High temperature down-hole environments; Electrical bulkhead feed-throughs.
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D1415
79
79
ASTM D2240
Tensile Strength, Yield 19.2 MPa
2780 psi
ASTM D412
Elongation at Break 131 %
131 %
ASTM D412
100% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Compression Set 26 %
26 %
72 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
CTE, linear 400 µm/m-°C

@Temperature 20.0 °C
222 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 325 °C
617 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: