Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 160 °C | 320 °F | short period, no load (dry sample) |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short period, no load (dry sample) |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
P & P Technology EC-J Silver Aluminum Loaded Silicone P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term |
Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term |
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term |
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term |
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | Intermittent |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | |
Sichuan Deyang Haton® hs12370 Polyphenylene Sulfide Coating Suspension; anti-corrosionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | a few hours operation |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | a few hours operation |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
ChevronTexaco FM NLGI 1 Grease EP FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term; EMS |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term; EMS |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term; EMS |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term; EMS |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | Intermittent |
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET) TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | Continuous |
Epoxy Technology EPO-TEK® B9021 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short term; EMS |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | |
BASF Sicotan® Yellow L 1916 Color Additive Description: Transparent yellow iron oxideChemical Structure: Iron Oxide HydrateSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdrying sys.. |
|||
Maximum Service Temperature, Air | 160 °C | 320 °F | short period, no load |
Omnia Plastica Omniamid PA6 G G - Dry Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |