Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
Mechanical Properties Metric English Comments
Tensile Stress 65.0 MPa
9430 psi
Elongation at Yield 7.0 %
7.0 %
7.0 %
7.0 %
flexural
Modulus of Elasticity 3.00 GPa
435 ksi
Flexural Strength 100 MPa
14500 psi
Flexural Modulus 2.50 GPa
363 ksi
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
flatwise; ISO 179 1fU
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Coefficient of Friction, Dynamic 0.090
0.090
Coefficient of Friction, Static 0.070
0.070
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
DIN 53752
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 120 °C
248 °F
160 °C
320 °F
short term
Vicat Softening Point 230 °C
446 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color slate grey