Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 140 °C | 284 °F | 20,000 hr; IEC 216 |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 H-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 140 - 150 °C | 284 - 302 °F | Short Term |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Mechanical |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Dynamic stressed parts.Isotrop.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
Lehmann & Voss LUVOCOM® 1/CF/15/TF/20/BK Polyamide 66, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short peaks operation |
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber 15% Glass fiber reinforced polypropylene for injection molding application.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short peaks operation |
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber 30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short peaks operation |
Polyram RamOfin PPH353M8 Polypropylene, 40% Mineral Filled 40% mineral filled polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | long term; EMS |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | 20000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | few hours; VDE 0304/P2-1, IEC 216 |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short Periods |
Hippe POM Copolymer Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | at 50% loss of tensile strength after 5000h; IEC 216-1 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short term |
CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber This material has good hot water resistance and sliding properties. Its applications include seals, scrapers and chain guides, and toothed wheels and rollers.Information provided by CENTROPLAST Eng.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | short term |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | Short term |
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | |
AlphaGary Evoprene™ Super G 947 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | UL746B RTI |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded
  AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |
|||
Maximum Service Temperature, Air | 140 °C | 284 °F | at 50% loss of tensile strength after 20000h; IEC 216-1 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |