Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 115 - 260 °C | 239 - 500 °F | Average value: 249 °C Grade Count:20 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica Akulon® PET Arnite Omnialite Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 20,000 hr; IEC 216 |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 W-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Electrical |
LE Phenolic Laminate Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many st.. |
|||
Maximum Service Temperature, Air | 115 - 240 °C | 239 - 464 °F | Average value: 155 °C Grade Count:4 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Continuous Use |
Polyram PlusTek PA602 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond 216C05 Information provided by Tra-Con Inc. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond 2170T Flexible Plastic Bonder TRA-BOND 2170T is a flexible, high viscosity, thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or alm.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive TRA-BOND CA-20 is a thixotropic epoxy adhesive system specially formulated for shorted turns, damaged end wire extensions, or other coil repair applications where a high-fill, non-sag adhesive is re.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Tra-Con Tra-Cast FS255 Flexible Clear Epoxy Casting Compound TRA-CAST FS-255 is a clear, low viscosity, epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties -- good clarity, long pot.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | short term; EMS |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Service |
3M FMV12 Void Polyester Label Products 3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Deflection Temp at unknown load |
Abatron AboCast 22-30/AboCure 50-12 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Service |
3M FMV01402 Triangle Void Polyester Label Products 3M™ Triangle Void Polyester Label Products FMV01202 and FMV01402 are a tamper-indicating stock designed to provide a triangle pattern in the facestock when removal is attempted. These label product.. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | |
Atom Adhesives AA-BOND F125 Epoxy Adhesive AA-BOND F125 is a 8 minutes gelling epoxy recommended for use in fiber optic connectors, optical and industrial bonding applications. AA-BOND F125 is clear, two part system is easily mixed and used .. |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Long Term |
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Maximum Service Temperature, Air | 115 °C | 239 °F | Long Term |
CENTROPLAST CENTROLYTE Polyethylene terephthalate This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote.. |