Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 20.0 - 24.9 W/m-K | 139 - 173 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Thermal Conductivity | 20.0 W/m-K | 139 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Thermal Conductivity | 20.0 W/m-K | 139 BTU-in/hr-ft²-°F | |
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology... |
|||
Thermal Conductivity | 20.0 W/m-K | 139 BTU-in/hr-ft²-°F | |
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORA.. |
|||
Thermal Conductivity | 20.0 W/m-K @Temperature 20.0 - 100 °C |
139 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Thermal Conductivity | 20.0 - 120 W/m-K | 139 - 833 BTU-in/hr-ft²-°F | in "ab" direction |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |