Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Super mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 243 PC 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic 1120 Corrosion-Resistant Panels Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASTHERM HT200 Insulation Sheet HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 125 PTFE, 35% Carbon Filled Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | |
3M Scotchcast™ 5400 Electrical Powder Resin 3M Scotchcast Electrical Resin 5400 has been specially developed for continuous coating process. It is well suited for applications where flexibility and resistance to cracking due to heat shock or .. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Thermal Conductivity | 0.270 W/m-K | 1.87 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Thermal Conductivity | >= 0.270 W/m-K | >= 1.87 BTU-in/hr-ft²-°F | ASTM C177 |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |