Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 85.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2 DN 70 is a ZTA Alumina Toughened Zirconia. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS327 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 15.0 - 16.6 W/m-K | 104 - 115 BTU-in/hr-ft²-°F | Z (vertical) direction, after mod H900 heat treat |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | Fiber Value |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |
|||
Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 - 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 20.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |