Polymer Property : CTE, linear = 46.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 83.0 µm/m-°C

@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
46.1 µin/in-°F

@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
NeXolve Clear Optionox® Polyimide Film/Coating
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 410 PC/PET alloy  (discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 410N PC/PET alloy, Flame Retardant  (discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
CTE, linear 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
Injection molded sample; ASTM D696
Ineos ABS Lustran® 356 Extrusion, Low-Gloss  (discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
CTE, linear 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
ASTM E831
BASF Capron® 8200 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
CTE, linear 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
ASTM E831
BASF Capron® 8202 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
CTE, linear 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
ASTM data
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)  (discontinued **)
Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination..
CTE, linear 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
ASTM data
BASF Capron® 8202 NL Nylon 6 (Dry)  (discontinued **)
Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 120H PC/ABS alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 130 PC/PBT alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 170 PC/PBT alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen)
Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang.
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
Absolute Drying; ASTM-D696
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-101 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-3000 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM E831
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
CTE, linear 83.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM Test
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 450N Polymer Alloy, Blow Molding
Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang.
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant
Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang
CTE, linear 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant
Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang