Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.0 - 57.6 µm/m-°C | 12.8 - 32.0 µin/in-°F | Average value: 43.9 µm/m-°C Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 132 Tin Solder Alloy High temperature electrical solderInformation Provided by Indium Corporation |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Global 508 30% Glass Filled PBT Gray Information provided by Global Polymers Corporation. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | Alpha 1 |
Lord Adhesives Thermosetâ„¢ ME-525 Underfill Encapsulant LORD Thermosetâ„¢ ME-525 encapsulant is a high purity, semiconductor grade epoxy underfill product developed for the encapsulation of flip chip devices. It is formulated to reduce warpage and wit.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy General purpose solderInformation Provided by Indium Corporation |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy Very good resistance to alkaline corrosionInformation Provided by Indium Corporation |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | ASTM D696 |
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | ISO 11359-2 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS303 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS304 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 23.0 µm/m-°C | 12.8 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 23.0 µm/m-°C @Thickness 1.60 mm |
12.8 µin/in-°F @Thickness 0.0630 in |
ASTM D696 |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
CTE, linear | 23.0 - 74.0 µm/m-°C | 12.8 - 41.1 µin/in-°F | Average value: 59.6 µm/m-°C Grade Count:24 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear | 23.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
12.8 µin/in-°F @Temperature -40.0 - 180 °F |
|
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
CTE, linear | 23.0 - 67.0 µm/m-°C | 12.8 - 37.2 µin/in-°F | Average value: 33.6 µm/m-°C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |