Material Notes:
General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 9.01 g/cc
0.326 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 16.5

@Load 4.00 kg
16.5

@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 43.4 MPa
6290 psi
Elongation at Break 20 %
20 %
% elongation on 5.65 (sq. root Area) gauge length
Thermal Properties Metric English Comments
Heat of Fusion 28.9 J/g
12.4 BTU/lb
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C
0.0399 BTU/lb-°F
Solid
0.201 J/g-°C
0.0480 BTU/lb-°F
Liquid
Thermal Conductivity 10.0 W/m-K

@Temperature 85.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 58.0 °C
136 °F
Eutectic
Solidus 58.0 °C
136 °F
Liquidus 58.0 °C
136 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 49 %
49 %
Indium, In 21 %
21 %
Lead, Pb 18 %
18 %
Tin, Sn 12 %
12 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000710 ohm-cm
0.0000710 ohm-cm