Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2:1999 |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
dry sample |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM D696 |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Ineos Nova S-5400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | Below Tg |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 100 °C |
44.4 µin/in-°F @Temperature 73.4 - 212 °F |
ASTM D696 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ASTM D696 |
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PA 6 C Nylon 6 Cast Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN132G15VO G/F Reinforced Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2; Parallel to Flow |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
D696 |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Duralco™ 4540 Machinable Epoxy Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: .. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 400H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X5402 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM E831 |
Addiplast Addinyl C2 R Nylon 66/6 High impact resistanceInformation provided by Addiplast. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
Dry; ASTM D696 |
Asahi Kasei Leona® 1300S Nylon 66 General purpose grade. Good balance of flowability and mechanical properties.Applications:Connectors, washers, cable ties. Information provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X5403 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM E831 |