Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.0 µm/m-°C @Temperature 23.0 - 100 °C |
41.7 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data) FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application.. |
|||
CTE, linear | 75.0 - 97.0 µm/m-°C | 41.7 - 53.9 µin/in-°F | Average value: 85.0 µm/m-°C Grade Count:7 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
CTE, linear | >= 75.0 µm/m-°C @Temperature 60.0 - 60.0 °C |
>= 41.7 µin/in-°F @Temperature 140 - 140 °F |
Average value: 75.0 µm/m-°C Grade Count:1 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear | 75.0 - 790 µm/m-°C | 41.7 - 439 µin/in-°F | Average value: 294 µm/m-°C Grade Count:20 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LI-941 ASA, Extrusion, High Heat Resistance Information Provided by LG Chem |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5404 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 6201 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant Information Provided by LG Chem |
|||
CTE, linear | 75.0 - 110 µm/m-°C | 41.7 - 61.1 µin/in-°F | ASTM D696 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 100 °C |
41.7 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ CA1110/2AC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact.. |
|||
CTE, linear | 75.0 - 80.0 µm/m-°C @Temperature 0.000 - 80.0 °C |
41.7 - 44.4 µin/in-°F @Temperature 32.0 - 176 °F |
ASTM D696 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
CTE, linear | 75.0 - 80.0 µm/m-°C @Temperature 0.000 - 80.0 °C |
41.7 - 44.4 µin/in-°F @Temperature 32.0 - 176 °F |
ASTM D696 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 526M02 High Tg Fiber Optic Adhesive TRA-BOND 526M02 is a two-part, low viscosity epoxy system that was developed specifically for fiber optic applications. This material is recommended for bonding fiber optic bundles, potting glass fi.. |
|||
CTE, linear | 75.0 - 85.0 µm/m-°C | 41.7 - 47.2 µin/in-°F | |
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive Ablebond 862-2 room temperature curing epoxy adhesive is designed for solder pad encapsulation or sealing the head/disk area in floppy disc assemblies. This resilient compound is suitable for bondin.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | ASTM D696 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 300Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5450 High Impact Polystyrene
(discontinued **) High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 40.0 - 130 °C |
41.7 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 100 °C |
41.7 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer Description: Hostacom™ ZB752AC precolored, medium melt flow, 2,800 MPa flexural modulus, mineral-filled polypropylene homopolymer has a very good combination of strength, stiffness, and impact resi.. |