Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 - 100 °C |
16.7 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 - 100 °C |
16.7 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2010 Cotton Fabric, Phenolic Resin Impregnated, Fine Application: slippers, inserts for coupling boxes, rollneck bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 - 100 °C |
16.7 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2040 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: slippers, gear-rods, bushesInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 30.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-3520F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high flowability realizes a thin w.. |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX CRN530 PPE+PA6 (Asia Pacific) 30%GF GTX grade for Non Auto market |
|||
CTE, linear | 30.0 - 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2949 PPE+PS (Asia Pacific) PPE+PS GF+Mineral Filler total 40% |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
CTE, linear | 30.0 - 35.0 µm/m-°C | 16.7 - 19.4 µin/in-°F | |
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperature.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and f.. |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® G-3420R Glass Fiber Reinforced Polycarbonate Resin GF 20% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |