Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Oxford Polymers 10GF 10% Glass Fiber Reinforced ABS, Flame Retardant 10% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
PTS PCA-30G00 Impact Modified Polycarbonate/PBT Alloy For Cold Temperature Impact.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000MDHL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO TL2 MB Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/ABS 1120 GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO TL20 LE Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A110 ABS, 10% Glass Fiber Reinforced Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed; ASTM D648 |
Techmer ES Plastiblend® ABS 922 NAT Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000MD5L Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant (5%)Features: LubricatedForm: Pellets Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
Oxford Polymers H-Acetal 20PTFE 20% PTFE Reinforced Homopolymer Acetal
(discontinued **) 20% PTFE Reinforced Homopolymer AcetalInformation provided by Oxford Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | Annealed; ASTM Data |
Styron Magnum™ AG700 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |