Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C @Thickness 3.18 mm |
331 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | |
Reliance Industries PBT / PC - 35% Glass filled Information provided by Reliance Industries |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plenco 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C @Thickness 3.20 mm |
331 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C @Thickness 3.20 mm |
331 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C @Thickness 3.20 mm |
331 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp GX05053 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX05053 is a compound based on Polysulfone blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plenco 7203 Phenolic, Granular, Transfer Molded PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 204 °C | 331 - 399 °F | ASTM D648 |
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6 Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7000 is the replacement material for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | ASTM D648 |
Plaslok 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 304 is a two-stage, woodflour and cel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 331 °F | As molded; ASTM D648 |
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 - 260 °C | 331 - 500 °F | Average value: 196 °C Grade Count:9 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |