Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 65H PC/ABS-Blend Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East) Lexan Copolymer resin with improved chemical resistance, available only in limited colors. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Diameter 6.35 mm |
226 °F @Diameter 0.250 in |
bar; ASTM D648 |
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.18 mm |
226 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Not Annealed; ASTM D648 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.17 mm |
226 °F @Thickness 0.125 in |
ASTM D648 |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5500EX PBT+PC (Asia Pacific) Non-FR, non-UV PC/PBT blend for film extrusion application |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO X Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO X MB Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® POM CO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PBT 03003 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | 0.5 inch unannealed; ASTM D648 |
PlastxWorld CEVIAN® VGR30 30% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | ISO 75-1/-2 |
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | ISO 75-1,-2 |
Covestro Bayblend® T85 SG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | annealed; ISO 75 |
Chi Mei Wonderloy® PC-385 PC/ABS Alloy Ultra-high Heat, Ultra-high Impact |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 108 °C | 226 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 1100 Tungsten Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc. |