Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 - 160 °C | 200 - 320 °F | Average value: 120 °C Grade Count:27 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF20 FR RD073 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Flame RetardantAppearance: RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF15 15% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF50 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Techmer ES Plaslube® NY-1/TF/12 Nylon 66, 12% PTFE Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 - 204 °C | 200 - 400 °F | ASTM D648 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C.. |