Category | Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Fluorosint® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.27 g/cc | 2.27 g/cc | ASTM D792 |
Water Absorption | 0.10 % | 0.10 % | Immersion, 24hr; ASTM D570(2) |
Deformation | 0.20 % | 0.20 % | 2000 psi; 122°F (50°C) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 74 | 74 | ASTM D785 |
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Elongation at Break | 40 % | 40 % | ASTM D638 |
Tensile Modulus | 2.25 GPa | 326 ksi | ASTM D638 |
Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Compressive Strength | 23.4 MPa | 3400 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 1.72 GPa | 250 ksi | ASTM D695 |
Shear Strength | 17.9 MPa | 2600 psi | ASTM D732 |
Coefficient of Friction, Dynamic | 0.18 | 0.18 | dry vs. steel; QTM55007 |
K (wear) Factor | 403 x 10-8 mm³/N-M | 200 x 10-10 in³-min/ft-lb-hr | QTM55010 |
Limiting Pressure Velocity | 0.158 MPa-m/sec | 4500 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 54.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Flammability, UL94 | V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 1.0e+6 ohm | <= 1.0e+6 ohm | ANSI/ESD STM 11.11 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Acceptable | Acceptable | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 5 | 1-10, 1=Easier to Machine |