Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C @Thickness 6.35 mm |
195 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Edgetek® XT XT-500-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AS-1000 HI Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:High ImpactPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ISO 75A-1,-2 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 - 149 °C | 195 - 300 °F | Average value: 142 °C Grade Count:83 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
I. Stern PS2110 General Purpose Crystal Polystyrene Features:Moderately High Heat ResistanceUL Classification 94 HBExcellent Water ClarityApplicationsDisplaysHouse waresInformation provided by I. Stern & Co. Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PBT/ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Spartech SP-9050 Low Gloss ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C @Thickness 3.17 mm |
195 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Chase Plastics CP Pryme® ASA300 BK General Purpose (Utility) ASA Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | Annealed; ASTM D648 |
American Polymers API 375 Polystyrene API 375 is a general purpose polystyrene produced in pellet form for injection molding. API 375 has excellent strength and clarity as well as fast set-up properties.Applications: Used in the manufa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Engineered Polymer Solutions ABS 550 Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM-D-648-56 |
BCC Products MB 5000 Urethane Tooling Board MB 5000 is an extremely tough, high impact Urethane Plank, that can be used for metal forming as well as nickel plating mandrels. Features: excellent machinability, low dust emission, mostly shavin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 - 96.1 °C | 195 - 205 °F | Average value: 93.3 °C Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
Chase Plastics CP Pryme® PE100-LD2M General Purpose Low Density Polyethylene Information provided by Chase Plastics. |