| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet |
| Manufacturer | Spartech |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Spartech SP-9050 Low Gloss ABS Sheet.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 81 | 81 | ASTM D785 |
| Tensile Strength, Yield | 31.0 MPa | 4500 psi | ASTM D638 |
| Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
| Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
| Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
| Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
| 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 | |
| Falling Dart Impact | 40.7 J | 30.0 ft-lb | 73°F; ASTM D3029 |
| 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.6 °C | 195 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 16 % | 16 % | Gardner; ASTM D2523 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Flammability | Passes | MVSS (Motor Vehicle Safety Standard) 302 |