Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | ASTM D648 |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | |
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | DIN 53461 |
Polyram RamShine PVS701 AES, UV Stabilized UV stabilized injection molding AESInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 89.0 °C | >= 192 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Staramide Z1000XXC PA66, Injection Molded Staramide Z1000XXC is an UV Stabilized Polyamide 66 Injection Molding Resin (also known as R1000HI0944)Information provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LS Nylon 66 A general purpose Nylon 66, lubricated and heat stabilized for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | 120°C/h; ASTM D 648 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | ASTM D648 |
Resirene Resirene® HH-107 General Purpose Polystyrene Features:Medium FlowHigh HeatHigh Molecular WeightHigh ProductivityFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Thin Wall ApplicationsExtrusionGPPS/HIPS BlendsCD CasesCassette CasesInf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | ASTM D648 |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |