Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of gener.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Polimeri Europa EDISTIR N1461 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM Data |
BASF Capron® 8200CQ Blend Nylon 6 (Dry)
(discontinued **) Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Ineos ABS Lustran® 752 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
GRECO ISOPAK 540 ABS Resin Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ISO 75-2 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 104°C (219°F) annealed; ASTM Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 941 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SC 202LV General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SP6433 9710 Medium Impact Polystyrene Characteristics High flow Good toughness Good shine Available in various colors Processing Injection molding Extrusion Applications Pipes & profiles for wiring Beading for furniture and tables .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | DIN 53461 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ISO 75-2 |
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Dow Retain® ABS 7490 ABS Data provided by Dow Chemical. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Ashley Polymers Ashlene® 526LD Nylon 66 Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M30L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |