Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ISO 75 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ASTM D648 |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | |
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ASTM D648 |
Spartech Polycast UF96 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific) LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® TN-1200 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 3.20 mm |
203 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
Method A; ASTM D648 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Method A - Annealed; ASTM D-648 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ISO 75-1, 2 |
Polyplastics Duracon® EB-10 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy Unique PC/ABS/SMA alloy with improved processing and reduced plate-outAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
Method A; ASTM D648 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |